Cut the board with board cutter into quarter. The patch part of the antennas then were coloured with black market or any colour but permanent marker. Wait until the marker dried up. If not, the ink will stick to the board and will damaged the board. Below are the process both for 8.5 GHz and 9.5 GHz.
- The plastic cover on the board was removed in *dark room and the transparency film was put on the board.
- The board then was put in the UV box for 237 sec to soften the photoresist that is not covered by black film in the shape of the patch.
* Had to remove in dark room in order to prevent the soften of the photoresist layer
Figure 1 : The UV box set to 237 sec
3. The board then is dipped in Sodium Hydroxide solution around 45 sec to 1 min until image developed and washed away the photoresist layer that was exposed to UV light. It will formed protective layer on the patch leaving the rest of copper exposed
Figure 2 : The board after dipped in Sodium Hydroxide
4. Then the board was rinsed with tap water.
5. Then the back of the board was suppose to be brush in order to remove the photoresist layer. But due to the scratch that will be left behind, other method was used. The technician of the Etching Lab told me that Thinner can be used. So there would not be any scratch. Only need to wipe a rag to the board. Using this way, the board will not be scratched.
Figure 3: The board when it was wiped with Thinner
6. Then the board was immersed in Ferric Chloride. This method will be the back site first then only the front side (where the patch was). The board will put on a hanger in order to quicken the process. If not using the hanger, it will take much longer time. The machine will do it's work. The temperature will be about 40 degree to 60 degree Celsius.
Figure 4 : The heated Ferric Chloride machine
7. The back side was put inside three times. Since one time is 4 min, the board was put 12 min. Then after the back side had completely removed the copper, the hanger was turned to the front side. The front side was also put 3 times, therefore 12 min too. Hence the total for 1 board was 24 minutes. After that, the board was taken out from the machine.
Figure 5: The board after taken out from the machine
8. The board then was rinsed with tap water.
9. The board front side was then wiped with Thinner to remove the clear dark yellow layer of photoresist on the patch.
Figure 6: The board after wiped with Thinner
10. Some parts on the board that was left with copper was then brushed with sandpaper to remove them.
11. The board was then drilled a hole to solder the connector (coaxial probe connector).
Figure 7 and 8 : The front and back view of 8.5 GHz microstrip patch antenna
Figure 9 and 10 : The front and back view of 9.5 GHz microstrip patch antenna
1. During the fabrication process, there had been many errors and damages done to the board. Initially, the board ordered was only for one board. Due to many damages done and many errors occurred during the process, 3 boards had been ordered in order to get the right results.
1.1 During this process, the first time doing this, the board was exposed to only 60 sec UV exposure. Making the image developed was so blurry. After the board was dipped in Sodium Hydroxide solution, the image developed was so thin making it like it will washed off. And the time taken to dip in Sodium Hydroxide solution took so long since the image developed was slightly thin :
1.2 The procedure was followed with the senior's methods. These methods were followed according to the senior's thesis. But following the instruction from the Etching Lad technician's the method used by the seniors written in the thesis were wrong. Therefore the process had to start again. This is from the senior's method:
1.3 This time around, the process were perfect, but the transparency film were not blackened with permanent marker making the square patch part were not solid rectangular and not perfect. It also had some scratches on it making it will be more losses when tested :
1.4 During the process to wipe the board with Thinner before immersing in Ferric Chloride, the rag that was used to wipe it contain some of the Thinner. Therefore, while holding the Thinner and wiping the board, some of the Thinner touch the patch part of the board (the front patch antenna part). Hence wiping some parts of
it :
1.5 During this process, there was a damaged done to one of the board. The marker that was coloured to the transparency film was not dried yet. The marker that stick to the board leave some marks to the board. The trails of the marker left behind made the patch of the antenna to become like this :
1.6 Other mistake includes the front patch of the antenna was touch with Thinner making some part of the patch missing :
1.1 During this process, the first time doing this, the board was exposed to only 60 sec UV exposure. Making the image developed was so blurry. After the board was dipped in Sodium Hydroxide solution, the image developed was so thin making it like it will washed off. And the time taken to dip in Sodium Hydroxide solution took so long since the image developed was slightly thin :
1.2 The procedure was followed with the senior's methods. These methods were followed according to the senior's thesis. But following the instruction from the Etching Lad technician's the method used by the seniors written in the thesis were wrong. Therefore the process had to start again. This is from the senior's method:
1.4 During the process to wipe the board with Thinner before immersing in Ferric Chloride, the rag that was used to wipe it contain some of the Thinner. Therefore, while holding the Thinner and wiping the board, some of the Thinner touch the patch part of the board (the front patch antenna part). Hence wiping some parts of
it :
1.7 Even though the right patch had been made, the board was cut a little smaller than it suppose to be:
No comments: